Feb 28, 2024 #1 Hajiwaji Mechanical Joined Jan 1, 2023 Messages 24 Location SA For caustic environment containing H2S and meet the definition of sour as per NACE MR 0103, does require testing and qualification for ssc? N06040 is not listed in NACE MR 0103 section 14.
For caustic environment containing H2S and meet the definition of sour as per NACE MR 0103, does require testing and qualification for ssc? N06040 is not listed in NACE MR 0103 section 14.
Mar 1, 2024 1 #2 SJones Petroleum Joined Apr 22, 2001 Messages 3,944 Location GB Check 14.1.1.2 against the base requirements for A494 N06040. Then review clause 11. Steve Jones Corrosion Management Consultant http://www.linkedin.com/in/drstevejones All answers are personal opinions only and are in no way connected with any employer. Upvote 0 Downvote
Check 14.1.1.2 against the base requirements for A494 N06040. Then review clause 11. Steve Jones Corrosion Management Consultant http://www.linkedin.com/in/drstevejones All answers are personal opinions only and are in no way connected with any employer.
Mar 3, 2024 Thread starter #3 Hajiwaji Mechanical Joined Jan 1, 2023 Messages 24 Location SA Thank you Dr. Jones. N06040 does not meet the chemical composition requirements in clause 14.1.1.2 of NACE MR 0103, hence qualifications are required as per clause 11. Upvote 0 Downvote
Thank you Dr. Jones. N06040 does not meet the chemical composition requirements in clause 14.1.1.2 of NACE MR 0103, hence qualifications are required as per clause 11.