6" schedule 80 (0.432) pipe, circumferential weld. A106, probably grade B. Weld made in standard fashion, E7018 fill passes.
Side 1: Carbon equivalent (per IIW) = 0.30; maximum HAZ hardness = 185 HV1 (1kg) ~90HRB
Side 2: CE = 0.40; maximum HAZ hardness = 180 HV1 ~89HRB
Any opinions on whether this weld was PWHT (required for service, not by Code)?? I cannot decide.
"If you don't have time to do the job right the first time, when are you going to find time to repair it?"
Side 1: Carbon equivalent (per IIW) = 0.30; maximum HAZ hardness = 185 HV1 (1kg) ~90HRB
Side 2: CE = 0.40; maximum HAZ hardness = 180 HV1 ~89HRB
Any opinions on whether this weld was PWHT (required for service, not by Code)?? I cannot decide.