We are needing to weld three to four topsides riser joints from X-65 line pipe, using FCAW-GS process (tig root). FCAW-GS consumable is lincoln 81-K2-H. Pipe size is DN700 x 39 mm wall thickness. Code is B31.8 which generally refers you back to API 1104.
At this thickness we need to PWHT. We are finding that the PWHT is degrading impact properties at the required -29 C and can't qualify the procedure. I am wanting to waiver the PWHT under clause A825 of B31.8 which permits this if we can demostrate that residual stresses are OK in the as welded condition. I believe CTOD's will justify such a waiver. However the A$20,000 this will cost us to run and test in australia does not make it cost effective for 3 or 4 welds. I am looking for a precedent or tech paper that has shown adequate as-welded properties for FCAW-GS on X65 line pipe in the past. Can anyone assist?
At this thickness we need to PWHT. We are finding that the PWHT is degrading impact properties at the required -29 C and can't qualify the procedure. I am wanting to waiver the PWHT under clause A825 of B31.8 which permits this if we can demostrate that residual stresses are OK in the as welded condition. I believe CTOD's will justify such a waiver. However the A$20,000 this will cost us to run and test in australia does not make it cost effective for 3 or 4 welds. I am looking for a precedent or tech paper that has shown adequate as-welded properties for FCAW-GS on X65 line pipe in the past. Can anyone assist?