Hi All,
The company I'm currently working for are manufacturing an accumulator vessel to ASME Section 3, NC.
I'm wondering if somebody can point me in the right direction, I'm looking to find out the qualification requirements for personnel visually inspecting welds on the above accumulator.
My train of thought is as below but I'm not totally convinced:
Section 3 NB - NB5000 Examination > NB-5521 Qualification - states shall be qualified in accordance with SNT-TC-1A.
NB-5111 > Refers me to Section 9 of ASME which again in the general requirements Article 1 says ASNT-TC-1A or ASNT CP-189.
So going form the above am I correct in assuming the visual inspectors on the job must be qualified in accordance with ASNT-TC-1A?
Look forward to hearing from some of you more experienced folk!
Thanks
The company I'm currently working for are manufacturing an accumulator vessel to ASME Section 3, NC.
I'm wondering if somebody can point me in the right direction, I'm looking to find out the qualification requirements for personnel visually inspecting welds on the above accumulator.
My train of thought is as below but I'm not totally convinced:
Section 3 NB - NB5000 Examination > NB-5521 Qualification - states shall be qualified in accordance with SNT-TC-1A.
NB-5111 > Refers me to Section 9 of ASME which again in the general requirements Article 1 says ASNT-TC-1A or ASNT CP-189.
So going form the above am I correct in assuming the visual inspectors on the job must be qualified in accordance with ASNT-TC-1A?
Look forward to hearing from some of you more experienced folk!