ASME B31.3-F308.2 state that "The need for venting the space between the welds in double-welded..."

Please help me in clarification it. Is this mean drill a hole for venting during welding? And after that is need weld to close it?

Thanks,
nlgcode
 
Replies continue below

Recommended for you

Read the section. If you need to leak check the inner fillet, you need a means to do that. It's of no use if you plug it. Appendix F is precautionary, not mandatory.

The predrilled vent hole is also helpful to ensure that you don't blow out a bubble in the closing (back) fillet due to expansion of trapped gas in the space between the two fillets.
 