Hello, I would like to know the UTS and Allowable shear stress values for Carbon Steel ASTM A350 LF2, at a temperature of 750F.

Thanks.
 
How about this approach, the allowable stress for ASME SA 350 LF2 at 750 deg F is 14.8 Ksi (per ASME B&PV Code, Section II, Part D). At 750 deg F, the allowable stress above is controlled by time dependent effects - like creep deformation. If your calculated stresses are at or below this value, you should be fine with plenty of design margin.
 
A350 Gr Lf2 is the fitting material for "LOW" temp. service. Where are you using this with such a high temp?
 