The dual certified material is used for procedure qualification (PQR) and the PQT has been passed. The material is certified to both A 36 (assigned as Group No I as per AWS D1.1 and P No. 1 as per Sec IX) and S275JR (classified as unassigned material as per both codes).
whether this PQR can be qualified to weld;
1. Both Group No I to Group No. I in the case of AWS D1.1 or P No.1 to P No.1 in the case of ASME Sec IX and the specific unassigned material (S275JR)?.
or
2. Only one material can be documented for PQR and the limit is applicable only for the documented material?. i.e if A36 is documented, then a new qualification is required to weld S275JR or vice versa.
You are all most welcome to share your knowledge with the reference code.
whether this PQR can be qualified to weld;
1. Both Group No I to Group No. I in the case of AWS D1.1 or P No.1 to P No.1 in the case of ASME Sec IX and the specific unassigned material (S275JR)?.
or
2. Only one material can be documented for PQR and the limit is applicable only for the documented material?. i.e if A36 is documented, then a new qualification is required to weld S275JR or vice versa.
You are all most welcome to share your knowledge with the reference code.