We need to protect a steel structure of approx 5m high that takes a load of 22T and is in a marine enviroment.
Hot dip galvanising seems to be the classic solution, but considering the size of the structure this causes some problems with the sub-contactors our client has approved(!!)
Is there a paint based process that can be used w/o baking that can produce a similiar level of protection.
Many thanks for your help
Hugh
Hot dip galvanising seems to be the classic solution, but considering the size of the structure this causes some problems with the sub-contactors our client has approved(!!)
Is there a paint based process that can be used w/o baking that can produce a similiar level of protection.
Many thanks for your help
Hugh