SA-240, Type 201 14 gauge stainless steel blanks are rolled and welded (autogenous) on a Jetline seam welder. This becomes the shell to which heads (SA-240, Type 304) are autogenously welded to make autoclaves.
One shell is 9" in diameter with a 12" long weld seam. Another shell is 11" in diameter with a 14.5" weld seam. The entire perimeter of both shells is blanked on a die and washed prior to welding.
We are experiencing periodic weld cracking on the larger shell's long seam. The crack is just under 3/16" long, located at the centerline of the weld bead, approximately half way along the length. When a crack appears, it is always in the same location.
Both shell blanks come from the same heat of material. Both blanks are processed identically. The burr from the die is controlled and is the same for both blanks. Yet we only experience cracking on the larger blank. The only difference that can be seen is the sheared edge has a rougher appearance on the larger blank.
This appears to be some kind of contamination issue. But why does it only occur on the larger shell?
Any thoughts are appreciated.
grayseal
One shell is 9" in diameter with a 12" long weld seam. Another shell is 11" in diameter with a 14.5" weld seam. The entire perimeter of both shells is blanked on a die and washed prior to welding.
We are experiencing periodic weld cracking on the larger shell's long seam. The crack is just under 3/16" long, located at the centerline of the weld bead, approximately half way along the length. When a crack appears, it is always in the same location.
Both shell blanks come from the same heat of material. Both blanks are processed identically. The burr from the die is controlled and is the same for both blanks. Yet we only experience cracking on the larger blank. The only difference that can be seen is the sheared edge has a rougher appearance on the larger blank.
This appears to be some kind of contamination issue. But why does it only occur on the larger shell?
Any thoughts are appreciated.
grayseal