Dear Experts,

Please help. why does the ASME SEC 9, in there material list with correspond to P-no (parent number) & group Number, that some materials are not listed. what is the reason why does those material are not included in ASME SEC 9 QW-422
In my case.. Im using ASTM A707 it is not included in list... so it means it is not C-MN carbon Manganese group-as per P1 material.. please enlighten
 
Replies continue below

Recommended for you

Please do not cross post. A response has been posted in thread330-393789.

 