212197, often for a welded joint the tube is lightly rolled to set the tube, then welded. This allows gases generated by welding to exit the joint on the shellside, helping to insure a sound weld. The tube may then be fully expanded, except for a margin at the weld itself and at the shellside.
This is what your detail appears to show.