Sirs
Can anybody suggest any reference for bond stress as per ACI-318..
i want to calculate the bond strength of anchors is tension. Since I don't have any America code reference, I am using BS8110-1 Clause 3.12.8.4.
ultimate Bond stress, Fbu = β Sqrt(Fcu).
We are using 4000psi Concrete, cylindrical strength f'c= 4000psi = 27.57 Mpa
Since we are using formula from BS, The Fcu Value should be cubic. therefore I will convert my
cylindrical strength to cubic strength
Fcu = f'c / 0.8 = 27.57 /00.8 = 34.46 Mpa. (β = 0.28 for plain bars)
Fbu = 0.28 x Sqrt (34.46) = 1.64 Mpa.
In the procedure ok, kindly advise..
Can anybody suggest any reference for bond stress as per ACI-318..
i want to calculate the bond strength of anchors is tension. Since I don't have any America code reference, I am using BS8110-1 Clause 3.12.8.4.
ultimate Bond stress, Fbu = β Sqrt(Fcu).
We are using 4000psi Concrete, cylindrical strength f'c= 4000psi = 27.57 Mpa
Since we are using formula from BS, The Fcu Value should be cubic. therefore I will convert my
cylindrical strength to cubic strength
Fcu = f'c / 0.8 = 27.57 /00.8 = 34.46 Mpa. (β = 0.28 for plain bars)
Fbu = 0.28 x Sqrt (34.46) = 1.64 Mpa.
In the procedure ok, kindly advise..