Hi can anyone tell me is there a ASTM standard (or other published standards e.g. ISO) for UHMW-PE pipe ?
 
Replies continue below

Recommended for you

D4020 is just the material spec for extrusion materials, not for pipe. It does not provide physical properties information requirements such as hydrostatic design base (HDB), tensile strength, etc. to determine the wall thickness required for pressure containment. Is there such a standard (similar to ASTM D3035 for PE pipe) for UHMW PE pipe from any standards organization ?
 