Hi All,
The team that I work with is require to buy a HNBR seal.
The vendor has provided us with 1 catalogue with the test values given (attached).
I am interested to know about the immersion test. I have downloaded the required ASTM (471 and 5964) for my references.
2 questions I want to ask :
1. How and where can I compare the typical value for HNBR under ASTM IRM 903 Oil?
2. The typical value for immersion test usually come with a (+/-) sign. What does this mean and how should it be correlated?
Thanks for the explanation in advance.
Cheer,
Jeffrey
The team that I work with is require to buy a HNBR seal.
The vendor has provided us with 1 catalogue with the test values given (attached).
I am interested to know about the immersion test. I have downloaded the required ASTM (471 and 5964) for my references.
2 questions I want to ask :
1. How and where can I compare the typical value for HNBR under ASTM IRM 903 Oil?
2. The typical value for immersion test usually come with a (+/-) sign. What does this mean and how should it be correlated?
Thanks for the explanation in advance.
Cheer,
Jeffrey