Greenleader
Aerospace
- Aug 10, 2004
- 68
Would the addition of tungsten, .55%, to 4340 mod, (300m),contribute a few points of hardness after tempering to spec?
I would like to add a little hardness without sacrificing strength or toughness or reducing the draw temp.
I would like to add a little hardness without sacrificing strength or toughness or reducing the draw temp.