Hi All,

I have a PQR (Charpy tested) and a WPS with a qualification range of 3mm to 12mm. My question is: I need to perform tube-to-tubesheet welding—can this PQR/WPS be used to cover the welding, referencing the code for the mock-up test? In that case, is a PWPS required for the mock-up test?

ps client’s spec doesn’t mentioning anything about tube to tubesheet welding apart referring to the code

Thanks
 
1) Talk to the client.
2) The manufacturer is responsible, you must have good technical judgment.

Regards
 
Solution
This depends on the code of construction:
e.g.
ASME VIII/2, 6.3.4 require qualification acc. to QW-193 (mock-up test)
"6.3.4 QUALIFICATION OF WELDING PROCEDURE
Tube-to-tubesheet welding procedure specifications shall be qualified in accordance with the requirements of Section IX, QW-193."

ASME VIII/1 do not require for Tube-to-Tubesheet Welds qualification the use of QW-193 except, if Tube-to-Tubesheet Welds
acc. to fig. UW-20.2(f) to (i) are used. For these joints mock-up qualification is required by note (3) to this fig.

For all other tube-to-tubesheet welds within the scope of ASME VIII/1, follow ASME IX, QW-202.6, which means that for pressure-retaining tube-to-tubesheet welds you have two options:
(a) groove welds per the requirements of QW-202.2 (Qualification for Groove Full Penetration Welds) and QW-202.4 (Dissimilar Base Metal Thicknesses)
(b) a demonstration mockup per the requirements of QW-193.1
 