Hi.
there is a shell & tube heat exchanger that shell side fluid is in severe wet sour service (HIC serrvice).
Tube & Tube Sheet material are carbon steel.
What kind of requirement for carbon steel was applied?
According to NACE PUB 8x194, there is no requirement for carbon steel tubing (for tube) & forging (for tube sheet).
Or gernral requirement shall be applied as per NACE MR0175.
Or just Killed Carbon Steel is no problem.
I'm very confused...
I would appreciate it if you explain the reason, additionally.
thanks for reading.
Regards,
there is a shell & tube heat exchanger that shell side fluid is in severe wet sour service (HIC serrvice).
Tube & Tube Sheet material are carbon steel.
What kind of requirement for carbon steel was applied?
According to NACE PUB 8x194, there is no requirement for carbon steel tubing (for tube) & forging (for tube sheet).
Or gernral requirement shall be applied as per NACE MR0175.
Or just Killed Carbon Steel is no problem.
I'm very confused...
I would appreciate it if you explain the reason, additionally.
thanks for reading.
Regards,