Apr 1, 2003 #1 JAYMON Mechanical Joined Apr 1, 2003 Messages 4 Location US Not cutting well at this point. Lots of dross and melting. Anyone with some suggestions....Using a 1500 mazak with the smart 3 system ,by the way...Thanx
Not cutting well at this point. Lots of dross and melting. Anyone with some suggestions....Using a 1500 mazak with the smart 3 system ,by the way...Thanx
May 1, 2003 #2 QSF Industrial Joined Jan 10, 2003 Messages 21 Location US Usually I will etch the part w/low power to burn thru the paint then i will cut it at a slightly slower speed than normal. Gary L. Ellis Jr. Quality Steel Fabrication Sidney, OH gellis@woh.rr.com Upvote 0 Downvote
Usually I will etch the part w/low power to burn thru the paint then i will cut it at a slightly slower speed than normal. Gary L. Ellis Jr. Quality Steel Fabrication Sidney, OH gellis@woh.rr.com