ctech,
In order to answer this question, you need to know what the thickness (minimum and maximum) of the coating is. If you are responsible for engineering this fastener and coating, then specifying an appropriate coating standard is necessary. This will provide details on the coating type, thickness, testing and inspection methods, etc. I am unclear what you mean by "hot solder dipping", so I cannot provide you with any more information.