I have an object 3D printed with plastic PLA, I want to painting it (with several colors) and then add a transparent coating to make my object conductive. Does anyone here have any experience with transparent conductive spray coating ?
 
Transparency and conductivity are typically mutually exclusive. So you need to decide how transparent and how conductive you need.

TTFN
I can do absolutely anything. I'm an expert!
faq731-376 forum1529
 
About the transparency, the coating should not spoil the paint.
About the conductivity, resistivity could between 106 and 109 ohms per square.
 
Ohms per square what? Guess over three orders of magnitude, it doesn't matter much.

Transparent conductive coatings do exist (what is that- indium oxide they use on solar panels?), but not out of a spray bottle. But what you need sounds like it's only conductive enough to be static dissipative, not really conductive per se, and maybe that stuff Mcvyvr recommended will do that.
 
the resistivity in ohms per square is independent of lateral dimension, since the effective thickness is what's important, and that's factored into the resistivity. That means that a 1 mm x 1 mm square has the same resistance as a 100 mm x 100 m square.

TTFN
I can do absolutely anything. I'm an expert!
faq731-376 forum1529
 
Thanks for clarifying IRStuff! It's a weird unit like mhOs I guess!
 