sparky1976
Electrical
Dear Forum,
I've tried to find the similar trhead but unfotunately there is no thread discussing this matter.
We have 150 kV transmission line double circuit distance 16 km with average load 110 MW.
Recently we experinced flash over on some of ceramic insulator and trips both lines, the weather was misty rain and foggy.
For short term remedy we wash (energized wash) the ceramic insulator.
For long term remedy I still need more input.
The suspect of this event are : changing season from long dry season to wet season, the line near(you can see the coast line from the towers)wind with salty water from sea.
My option are :
1. add more ceramic insulator
2. coating with silicone which I already proved not make any improvement with my MV O/H line right near the sea, and the coating will peeled if we do the energized washing.
3. Chopper energised washing.
Is any one on the forum experince similar problem ?
If any one has some suggestion ?
I'm scraching my head,pulling my hair this last couple weeks to find good resolution to make sure this not happen again.
Thanks
Pitat
I've tried to find the similar trhead but unfotunately there is no thread discussing this matter.
We have 150 kV transmission line double circuit distance 16 km with average load 110 MW.
Recently we experinced flash over on some of ceramic insulator and trips both lines, the weather was misty rain and foggy.
For short term remedy we wash (energized wash) the ceramic insulator.
For long term remedy I still need more input.
The suspect of this event are : changing season from long dry season to wet season, the line near(you can see the coast line from the towers)wind with salty water from sea.
My option are :
1. add more ceramic insulator
2. coating with silicone which I already proved not make any improvement with my MV O/H line right near the sea, and the coating will peeled if we do the energized washing.
3. Chopper energised washing.
Is any one on the forum experince similar problem ?
If any one has some suggestion ?
I'm scraching my head,pulling my hair this last couple weeks to find good resolution to make sure this not happen again.
Thanks
Pitat