Is it correct to say that with TMCP steels being rolled at various temperatures and in various directions(???) - that rolling direction is no longer an issue for cold forming of a TMCP plate?
 
Replies continue below

Recommended for you

Rolling direction is not as much of a concern with many steel types, now that clean steel processing has reduced inclusion contents. The following is a nice description from Stu Keeler, forming guru: