Yes, microscopy, either manual (tedious!) or automated can determine the fraction of ferrite, so long as the etch clearly differentiates the phases. Ferrite in martensitic SS is white in micrographs I have seen.
Impact testing is a crude, qualitative way to compare ferrite content in samples.