I have a part which i'm supposed to get a quote from tooling supplier and also making unit price. I just need some pointers on the important areas that i have to focus on regarding tool design and moulding the part so i can estimate the level of difficulty in making this tool and producing the parts.
I'd love to attached the drawing but i'm not sure if its allowed. Anyways, the design of the part is simple:
- Imagine a rectangular container without the top cover.
- Height 5.4mm, length: 59.5mm, Width: 20mm
- Part thickness : 0.17mm-0.2mm (i've double checked the drawings and it is 0.17mm. Please inform if its impossible to mould such thin parts)
- part weight: 0.34g
- Material: PC w/CBT(i'm not sure what CBT is at the moment)
- On the bottom plane of the part, its filled with about 50 small holes (0.64mm) in diameter.
My main worry is:
- is PC material suitable for such thin wall moulding?
- What type of gate and which position on the parts should it enter?.. smaller side of the part (20mm) or the larger side of the part (59.5mm)
- Important notes in thin wall moulding as in , should there be special inserts for venting, also important venting area in order to fill the parts efficiently.
I hope the question is clear. any comments would be appreciated.
thanks
Sizzerpac
Program engineer
I have a part which i'm supposed to get a quote from tooling supplier and also making unit price. I just need some pointers on the important areas that i have to focus on regarding tool design and moulding the part so i can estimate the level of difficulty in making this tool and producing the parts.
I'd love to attached the drawing but i'm not sure if its allowed. Anyways, the design of the part is simple:
- Imagine a rectangular container without the top cover.
- Height 5.4mm, length: 59.5mm, Width: 20mm
- Part thickness : 0.17mm-0.2mm (i've double checked the drawings and it is 0.17mm. Please inform if its impossible to mould such thin parts)
- part weight: 0.34g
- Material: PC w/CBT(i'm not sure what CBT is at the moment)
- On the bottom plane of the part, its filled with about 50 small holes (0.64mm) in diameter.
My main worry is:
- is PC material suitable for such thin wall moulding?
- What type of gate and which position on the parts should it enter?.. smaller side of the part (20mm) or the larger side of the part (59.5mm)
- Important notes in thin wall moulding as in , should there be special inserts for venting, also important venting area in order to fill the parts efficiently.
I hope the question is clear. any comments would be appreciated.
thanks
Sizzerpac