thread725-238462
referring back to this thread in regard to thickness i have a welder qualified on a two process pqr and another who is not - gtaw for root/hot pass
i was reffring to qw451 in my answer to the project manager with the proviso that furher info is req'd.
question is, can i use the gtaw only welder on the two process butt (its a 900dn) for the root and hotpass only, then wait till i get the other qualified welder back on the job to finish the butt. thickness qualified to was 5.54mm and 900 butt is 12.97.
i have also looked at qw356 and qw452.1b which seems to indicate that i can use the wedler only qualified to the gtaw process for 11.66 (or the first 3 runs on this butt)
thanks
 
Replies continue below

Recommended for you

verdiblue,
Your interpretation is correct (qualified weld metal thickness would however be 11.08 mm, not 11.66 mm).
Refer also QW 351 (paragraphs 3 & 4)
Regards,
DD
 
thats fantastic dekdee - just what i was looking for. thanks very much
 