Hi,

Trying to make a bathroom scale with a tempered glass top, but unsure how to calculate the required thickness for four, five or more contact points. Please advice.

-Simon
 
Replies continue below

Recommended for you

Do you have a good lawyer?

Just66horns
I changed the horns and now mine goes beep beep
 
use Roark to get an elastic stress and design accordingly.
 
limit tensile stresses to less than 1000psi or the glass can unpredictably fail due to "static" fatigue (ie subcritical crack growth). Your temper will make this difficult to calculate, but if you are selling this, you must do due dilligance.

be careful, glass does not like water (humiditiy included), beilieve it or not.
 