can anybody advice which NDT will be better for finding out the remaining thickness of A179 tubes of surface condenser?

Regards

Iqbal
 
Replies continue below

Recommended for you

I'd also vote for eddy current, but then scratched my head

-- franklin, aren't you replacing the entire tube bundle? Given the situation you first described, trying to replace individual tubes makes no sense.

At best, given your February outage, doing eddy current would allow you to derate and limp along until you can replace the entire tube bundle.

Patricia Lougheed

******

Please see FAQ731-376: Eng-Tips.com Forum Policies for tips on how to make the best use of the Eng-Tips Forums.
 
Your choices are eddy current or pulling a tube sample and sending it to a lab for testing.

If for some reason you can't do either one of those, you could get a machinist to try to get you an inside mic reading of the tube ID. Problem is, unless you had good records of what they tubes originally were, there might have been enough variation in the original tubes to throw off your ID readings.

rmw
 
VPL
We have decided to replace some of the tubes during Feb outage. The reason i s that the the new bundle delivery time s beyond February 2011.
Anyhow now we are adopting the same strategy of changing some tubes at bottom portion (the most vulnerable portion)and the remaining tubes will be replaced next year based eddy current results.
 