Can anyone tell me the outer diameter for THHN 16AWG? My NEC book only goes down to 14AWG.

Thx,
Tef
 
Replies continue below

Recommended for you


The closest equivalent for 16AWG fixture wire is TFN solid; TFFN stranded.
 
Thanks David! Sadly, I was at the Superior Essex site and didn't even see it. Guess I better get my eyes checked... [3eyes]

Tef

P.S. - Nice to see other EET's out there.
 
THHN is only readily available down to 14awg.....16awg and lower are manufactured as TFFN....for most manufacturers is actually the same insualtion and elastomeric cover, being that most wires are valued as more than one category.
Also, you will see the insulation value rise to 105C
 