Does anyone know of or has anyone seen a poster size reference chart that has among other things, the thermal coefficient of expansion for various materials? I believe there are also graphical representations of the material's deflection vs temperature for the pertinent range(s).
 
You can find the data that you are looking for by clicking on the link below.



This website contains a great deal of information about the properties of materials. The address given above lists the coefficient of thermal expansion for more than 3,000 materials. Good luck.
 
Be careful with TEx data. You have to watch what they are reporting. Is the number at a specific temp or over a range? Look carefuly.

= = = = = = = = = = = = = = = = = = = =
Corrosion never sleeps, but it can be slowed down.
 
I'm looking specifically for this poster rather than material properties. It has been years since I last saw one but I know what I'm looking for does exist.

There are many references where one can find characteristics for a given material; matweb is one of the least desirable choices.
 
"There are many references where one can find characteristics for a given material; matweb is one of the least desirable choices."

one question: Why do you consider matweb one of the least desireable choices?

nick
 
Published references are preferred. All information on the web is questionable.
 
"Published references are preferred. All information on the web is questionable."

true, however MatWeb is an exception (along with other places on the web). If you look at the bottom of the datasheet there is often a list of references given. Admittedly this data often has no test method given nor any info on various preperation procedures. Using that level of skepticism though the only desireable choice is the ASM Metals Handbooks, These are very expensive, and more than complete, however they are sure to contain an error or two.

Even the Guide to Engineered Materials published by ASM in AM&P every december has errors.

I gues I just havent found a fatal flaw yet in matweb and wonder if there really are any.

Not that I would use mat web as a certifiable source. That can only be done by an accreditted lab and or the producer of a material.

nick
 