I need help about one subject related to piping material selection.
For reasons of delivery time of the piping and accessories contractor asks to use LTCS instead of CS with impact test for the pipes greater or equal to 12.7 mm thickness, is it possible to use LTCS material instead of CS material within a T° range of -29°C to 340°C, instead of using CS material to avoid Impact test.
If for some reasons we want to keep the same material of valves (CS) those valves will be installed in LTCS lines but within the T° range stated above.
is there any corrosion problem if joining LTCS flanges with CS valves, what is the suitable bolting material that can be used.
Regards
For reasons of delivery time of the piping and accessories contractor asks to use LTCS instead of CS with impact test for the pipes greater or equal to 12.7 mm thickness, is it possible to use LTCS material instead of CS material within a T° range of -29°C to 340°C, instead of using CS material to avoid Impact test.
If for some reasons we want to keep the same material of valves (CS) those valves will be installed in LTCS lines but within the T° range stated above.
is there any corrosion problem if joining LTCS flanges with CS valves, what is the suitable bolting material that can be used.
Regards