The specification states that hot applied thermo-plastic materials shall be of such rthickness to uniformly coat the equivalent of 14mm single surface dressin g and having a minimum thickness of 3mm.But the manufacturer says that the road marking paint of 3mm thickeness is too thick.Please assist of this issue prior advising the Contractor.
 
Replies continue below

Recommended for you

thermoplastic and paint are 2 different things....... 3mm (1/8 ")is a fairly typical thickness for extruded thermoplastic markings.
 