QualityTime,
I don't know where to begin to correct you...
Mixed flow pumps run against a liner, though I'm not convinced this is even a mixed flow pump.
Blockages at the suction, cavitation, or increased clearance would be assoc. with high vibration and noise, which wasn't mentioned.
Forget looking into any bowls for trash... 10 stages and only 10 hp motor indicates these are very small bowls and impellers (even smaller hydraulic passages).... actually the curve shows the impellers are only 5" in diameter.
What is more likely, and I have seen in my many years of pump testing, is variations in castings (vane thickness and geometry) on the smaller impellers contribute to greater performance variations (+/- 1/4" deviation on a 5" dia impeller is a greater portion of the total area then on a 35" impeller).... or even more likely, the setup and test equipment in the field isn't ideal.
Did you know that 76.4% of all statistics are made up...