when reviewing a WPQ
SA 53 GRADE B PIPE ( TS-60,000 PSI) The Tensile test result indicate 56,900 psi broke in base metal.
5% of tensile strength below is 57,000 psi.
so it break in base metal at 57,000 psi will be accepted.
now if i get 56,900 what is result.?

 
You know the answer to this one.....unfortunately. [thumbsdown]
 
I agree with David; looks like a failure to meet the minimum specification requirements.

When I review such documents, I double check the math as the results could have been reported incorrectly. The rounding/number of significant figures used for the calculation could possibly, though unlikely, make a difference as well.
 
Yes , i also agree but i was told result is pass because of rounding numbers. so i didn't understand.
so i thought i will put this question to ask some experts about their opinion.
Regards
stanly
 
Think of it this way. The purpose of a procedure qualification is to prove that your welding procedures essential variables are established and will guide a welder to make sound welds. The purpose of a welder qualification is to prove the welder a ability to deposit sound weld metal. If either of these doesn't pass there is a reason. Most acceptable tensile tests on welded joints pass well beyond the minimum specified values. If you are trying to skirt past the requirements based on a rounding issue, then don't expect good results on your production welds. It's just not worth it.

API510,API570,API653,API577,API571,
API580, NBIC AI. A.S. Eng, BSME
 
Your measurements for determining area were no doubt to 3 significant figures; therefore the tensile results are to 3 significant figure and may not be rounded up to 57,000 (2 significant figures). But do check the math as per SectionIX. I would be more concerned with the low tensile results of the SA-53 B, especially if it is representative of material purchased for installation.
 
Inspect this specimen, may be machined wrong.

Regards
r6155
 