I am running a model simulating composite delamination using a cohesive interface. The model delaminates correctly using energy based damage evolution, however when I try to use displacement based, tabular data to define the softening curve, it does not delaminate. I am trying to implement a trapezoidal cohesive law. I have defined the tabular displacement by equating the area under the softening curve to the Fracture toughness (1.0755 N/mm) and am using MPa and mm.
Does anyone know why this is not delaminating? Or have experience implementing a trapezoidal cohesive law?
Thanks
** MATERIALS
**
*Material, name="Material 1"
*Elastic, type=ENGINEERING CONSTANTS
159000.,8490.,8490., 0.32, 0.32, 0.32,4610.,2780.
2780.,
**
** INTERACTION PROPERTIES
**
*Surface Interaction, name=Bonding
1.,
*Cohesive Behavior
3.52e+06, 2.78e+06, 2.78e+06
*Damage Initiation, criterion=MAXS
10000., 128.5,10000.
*Damage Evolution, type=DISPLACEMENT, softening=TABULAR
0., 0.
0.989, 0.0042
1., 0.0125
*Damage Stabilization
1e-05
Does anyone know why this is not delaminating? Or have experience implementing a trapezoidal cohesive law?
Thanks
** MATERIALS
**
*Material, name="Material 1"
*Elastic, type=ENGINEERING CONSTANTS
159000.,8490.,8490., 0.32, 0.32, 0.32,4610.,2780.
2780.,
**
** INTERACTION PROPERTIES
**
*Surface Interaction, name=Bonding
1.,
*Cohesive Behavior
3.52e+06, 2.78e+06, 2.78e+06
*Damage Initiation, criterion=MAXS
10000., 128.5,10000.
*Damage Evolution, type=DISPLACEMENT, softening=TABULAR
0., 0.
0.989, 0.0042
1., 0.0125
*Damage Stabilization
1e-05