Dear all ,
Table UG-84.6 Required HAZ Impact Test Specimen Set Removal
when Base Metal Thickness t ≤ 3/ 4 in. One set of HAZ Specimen in the Locations of Their Approximate Centerline 1/ 4 t to 1/ 2 t.
We got a laboratory test report following
1.Base Metal Thickness:4mm (SA-516 70)
2.v-notch Specimen for HAZ: 3.3 X 10 X 55 mm
question:
1. Is 3.3 MM acceptable for a 4t thin plate?
2. should we ask laboratory to re-make a HAZ v-notch Specimen at 1 X 10 X 55 mm ?
Table UG-84.6 Required HAZ Impact Test Specimen Set Removal
when Base Metal Thickness t ≤ 3/ 4 in. One set of HAZ Specimen in the Locations of Their Approximate Centerline 1/ 4 t to 1/ 2 t.
We got a laboratory test report following
1.Base Metal Thickness:4mm (SA-516 70)
2.v-notch Specimen for HAZ: 3.3 X 10 X 55 mm
question:
1. Is 3.3 MM acceptable for a 4t thin plate?
2. should we ask laboratory to re-make a HAZ v-notch Specimen at 1 X 10 X 55 mm ?