Dear Friends

Applicable Code- AWS D1.1. tEST pOSITION -6GR.
1)For full Mech. Test/Impact Energy-6GR-Mat. API 5L X52-Group II Mat used
2) For Macro - EH36-Group Material II used. In which clause as per AWSD1.1 it is allowed?
Appreciate prompt answer
 
Replies continue below

Recommended for you

Dear Friends
Is it mandatory or option to conduct Mock-Up Test( AWS D1.1-4.12.4.1) in qualifying PQR for 6GR-T-Y-K?