Apr 11, 2010 #1 4872 Petroleum Joined Jan 7, 2008 Messages 34 Location SG Dear Friends Applicable Code- AWS D1.1. tEST pOSITION -6GR. 1)For full Mech. Test/Impact Energy-6GR-Mat. API 5L X52-Group II Mat used 2) For Macro - EH36-Group Material II used. In which clause as per AWSD1.1 it is allowed? Appreciate prompt answer
Dear Friends Applicable Code- AWS D1.1. tEST pOSITION -6GR. 1)For full Mech. Test/Impact Energy-6GR-Mat. API 5L X52-Group II Mat used 2) For Macro - EH36-Group Material II used. In which clause as per AWSD1.1 it is allowed? Appreciate prompt answer
Apr 20, 2010 Thread starter #2 4872 Petroleum Joined Jan 7, 2008 Messages 34 Location SG Dear Friends Is it mandatory or option to conduct Mock-Up Test( AWS D1.1-4.12.4.1) in qualifying PQR for 6GR-T-Y-K? Thanks Upvote 0 Downvote
Dear Friends Is it mandatory or option to conduct Mock-Up Test( AWS D1.1-4.12.4.1) in qualifying PQR for 6GR-T-Y-K? Thanks