I worked as a engineer for the forging industry and came across a technology that will diffuse Titanium into tool steel substrate, H13 @ 46-48 Rc, and produce a 75 Rc surface, .005-.006 deep. This is done to finished, ready for production tooling. Does not change dimension or distort the finish tool.

Terry62
 
Do you mean nitriding?
 
No, I've tried Nitriding and made the tooling brittle. This method is Titanium diffusion. I accomplished this with finished tooling. With Nitriding, had to refit tooling, afterward.
 
No this process uses Ti in a gas phase (with Cl or F) and hot enough that the gas decomposes on the surface and you form TiC in reaction with C in the bulk alloy. I have done this on alloy cast iron. It does work.
I believe that was Union Carbide Coating Services that did it.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
No, Ed this is a liquid bath process, under tempering temperatures of tool steels. This process is done by Philos Technologies in Wheeling, IL. Check out: