I worked as a engineer for the forging industry and came across a technology that will diffuse Titanium into tool steel substrate, H13 @ 46-48 Rc, and produce a 75 Rc surface, .005-.006 deep. This is done to finished, ready for production tooling. Does not change dimension or distort the finish tool.
Terry62
Terry62