Can anyone recommend me a surface treatment for INCO 718 for use in wear , fatigue applications? Is passivation is enough?

Thanks in advance
Best reagards
 
Replies continue below

Recommended for you

What is the environment including temperature variations, type of abrasive likely to be encountered, etc.? For fatigue resistance, you don't want any type of coating, just the normal heat treating and cleaning recommended by Special Metals/Cartech/etc. For wear resistance, other considerations may need to be made.
 
For wear resistance you can try a hard PVD nitride, such as titanium nitride (TiN). For high temperature applications (over 500 C), titanium aluminum nitride (TiAlN) would be best. I'm not sure how the process will affect fatigue life for INCO 718.

Jim Treglio
 