Hello all,

It seems like there are quite the issue now and days with dichromate. Does anyone know what has replaced it in ASTM B633 standard? i do not have access to it. What has replaced it or equivalent that can pass Type VI with 120HR minimum Salt Spray pass?

FGY
 
Replies continue below

Recommended for you

There are inorganic zinc/aluminum flake products that are far superior to zinc chromate for corrosion resistance. An example trade name is Dacromet.
 