Oct 12, 2005 #1 MatEngTED Materials Joined Sep 27, 2004 Messages 24 Location US Need to locate supplier source(s) for polyvinyl butyral (PVB) phenolic film. Any recommendations appreciated.
Need to locate supplier source(s) for polyvinyl butyral (PVB) phenolic film. Any recommendations appreciated.
Oct 12, 2005 #2 Demon3 Materials Joined Jun 6, 2005 Messages 1,850 Location US PVB is not a phenolic resin so I am confused about your request. A quick google search shows DuPont and Wacker as PVB producers. They are global so ask them for your local dealer. Upvote 0 Downvote
PVB is not a phenolic resin so I am confused about your request. A quick google search shows DuPont and Wacker as PVB producers. They are global so ask them for your local dealer.
Oct 12, 2005 Thread starter #3 MatEngTED Materials Joined Sep 27, 2004 Messages 24 Location US The phenolic acts as a crosslinking agent. Upvote 0 Downvote
Oct 13, 2005 #4 Demon3 Materials Joined Jun 6, 2005 Messages 1,850 Location US Cool. Didn't know anyone cross-linked that polymer. By the way it's quite expensive stuff the PVB but you can get it used (recycled from cars) cheaply. I have a friend working with that. Upvote 0 Downvote
Cool. Didn't know anyone cross-linked that polymer. By the way it's quite expensive stuff the PVB but you can get it used (recycled from cars) cheaply. I have a friend working with that.