Bruce Wetmore
Industrial
I need to place a very flat concrete slab to be polished, but it must be placed in a room with 4 concrete walls, placed up to the wall edges to ultimately be polished to the wall edges.
We always used formwork to set levels, screed and tamp, but if it must be flush with concrete walls how can we screed and tamp?
Slab Thickness: 150 mm (6 inches).
Area: 8m x 12m (26 ft x 40 ft) rectangular room.
Great thanks for any advice!
We always used formwork to set levels, screed and tamp, but if it must be flush with concrete walls how can we screed and tamp?
Slab Thickness: 150 mm (6 inches).
Area: 8m x 12m (26 ft x 40 ft) rectangular room.
Great thanks for any advice!