stanweld99
Nuclear
For super duplex with impact test, and qualification code is in accordance with IX and B31.3, should the qualified wall thickness range follow SECTION IX or B31.3.
Since the charpy test (at -46°c) is not as required by ASME B31.3, my interpretation is that WPS qualified wall thickness range should follow SECTION IX.
I would like your input.
Thanks
Stanweld99
Since the charpy test (at -46°c) is not as required by ASME B31.3, my interpretation is that WPS qualified wall thickness range should follow SECTION IX.
I would like your input.
Thanks
Stanweld99