Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Structural Minimum thickness for Pipe sizes above 24" 1

Status
Not open for further replies.

Sarahm554

Materials
Joined
Oct 17, 2015
Messages
13
Location
AE
Hi,
Hope everyone is having a great time.
As we can see that API-574 (Table-6) dictates the structural minimum thickness for carbon and low alloy steel pipes but if the pipe size is more than 24" and MAWT is very low (even below the structural minimum of 24" pipe) then what criteria should be followed.
Thanks in advance
@SAhmad
 
Can you post the section of table 6 so we all understand what you're talking about please.

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
API 574 is a piping inspection standard.
It should not be used for design.

Check your design code for Max D/t limits.
Ensure that your resulting pipe thickness meets all other design loading conditions as specified in your design code.
Ensure that your resulting pipe thickness will be sufficient to prevent excessive ovaling during handling and transportation.

 

I think the subject table is table - 1 and copy and paste of the same,

API_NPS_etc_tzxzme.jpg


One can see that the minimum wall thickness 6.35 mm (1/4 in) when the size is greater than 8 in. and less than 36 in .

For cs pipe, the minimum thickness shall also satisfy a minimum resistance to handling damage, buckling,internal pressure external loading etc...

You may look the same ( API RECOMMENDED PRACTICE 574 ) section 12 Determination of Minimum Required Thickness....
 