Does anyone know where I can find stress strain curves for aluminum alloys, particularly 6005-T5?
 
Replies continue below

Recommended for you

Mil-Handbook-5/MMPDS-01/MMPDS-02. See various posts in the Aircraft Engineering forum for sources.
 
NO 6005???

MatWeb Data Sheet

Aluminum 6005-T5 Date: 11/15/2006 1:15:02 PM


KeyWords:
UNS A96005; ISO AlSiMg; Aluminium 6005-T5; AA6005-T5
"SubCat: Aluminum Alloy, Nonferrous Metal, 6000 Series Aluminum Alloy, Metal"
Material Notes:
"Data points with the AA note have been provided by the Aluminum Association, Inc. and are NOT FOR DESIGN."

Component Value Min Max
"Aluminum, Al" 97.5 99
"Chromium, Cr" 0.1
"Copper, Cu" 0.1
"Iron, Fe" 0.35
"Magnesium, Mg" 0.4 0.6
"Manganese, Mn" 0.1
0.05
 