How can I calculate the flexural stress in 3 foot square precast concrete pavers, due to 15 kip concentrated post load? Pavers are 3" thick and bear on 2" thick HL 60 polystyrene insulation, and 2" pea gravel material below that, then suspended reinforced concrete slab below (the suspended reinforced slab can be considered to be rigid relative to the paver).
A few years ago I wrote a spreadsheet of the Westergaard equations, to evaluate this type of situation, but I would like to have a check of that. There used to be a neat thing on the internet where you input he parameters and it showed the stresses, with load placed at mid-panel, at edge of panel and at corner. But I can no longer find that. Would anyone know where something like that might be on the internet?
Also is there any simple way of doing a finite element type of analysis to determine the stresses in the paver? If so, is there something explaining the method, so I could proceed to carry it out?
A few years ago I wrote a spreadsheet of the Westergaard equations, to evaluate this type of situation, but I would like to have a check of that. There used to be a neat thing on the internet where you input he parameters and it showed the stresses, with load placed at mid-panel, at edge of panel and at corner. But I can no longer find that. Would anyone know where something like that might be on the internet?
Also is there any simple way of doing a finite element type of analysis to determine the stresses in the paver? If so, is there something explaining the method, so I could proceed to carry it out?