Yes it depends on a lot of factors.
You have to make a bunch of assumptions; ductile materials, properties largely unchanged by welding, weld filler modestly stronger than base metal, loads a small fraction of ultimate, no high cycle fatigue, and so on.
Of course a lot of this goes away if they just use a full pen weld
= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed