Hi,
I would like to know if there is any documentation on the strength of laser weld. Is it about 80% of the material strength?

Regards.
 
Yes, there is enormous documentation in technical journals. You can perform a search at:


The strength varies so greatly with starting material and process parameters that stating a single value like 80% is inappropriate.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
If I'm using SS 17-4PH, what is a comfortable figure I can start with?

Regards.
 
What heat treatment does the starting material have? Do you perform any post-welding heat treatment? Unlike a simple low carbon steel, your material is quite complex, which means there is no comfortable figure without a complete description of the material condition and process parameters.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Hi Cory,
Thanks for the reply.
There will be a heat treatment process to H1075 before the laser welding process. There will not be any post-weld heat treatment.