Jul 23, 2012 #1 milena02 Agricultural Joined May 12, 2009 Messages 42 Location AR How is call a heat (cool) treatment for alumniniun, when after heated and quenched in water, it shall be put in a refrigeration chamber at a very low temp , at least -29ºC , to stop the Al. ageing. Material thicknes is about 0.125"
How is call a heat (cool) treatment for alumniniun, when after heated and quenched in water, it shall be put in a refrigeration chamber at a very low temp , at least -29ºC , to stop the Al. ageing. Material thicknes is about 0.125"
Jul 23, 2012 Thread starter #2 milena02 Agricultural Joined May 12, 2009 Messages 42 Location AR It is to sustain the AS QUENCHED state . Upvote 0 Downvote